该系统通过将冷却剂喷淋到移动的铸坯上来工作,分为多个区域。每个区域的流量、压力和喷淋模式独立控制,并根据铸造速度和合金自动调整。冷却剂均匀地提取热量,完成凝固并控制温度梯度,以最大限度地减少热应力。控制系统使用传感器和执行器来保持精确冷却,响应时间≤1秒,控制精度±2%。
| 参数 | 典型区间 | 选型说明与越界后果 |
|---|---|---|
| 冷却水流量 | 80–200 m³/h | Determines cooling intensity and billet surface temperature. |
| 水压 | 0.4–0.8 MPa | Affects spray atomization and cooling uniformity. |
| 喷嘴数量 | 120–240 pcs | More nozzles improve cooling uniformity. |
| 冷却区长度 | 3–6 m | Longer zones allow gradual cooling. |
| 铸坯温度范围 | 800–1100 °C | Typical surface temperature after secondary cooling. |
| 水温 | 20–35 °C | Higher temperatures reduce cooling efficiency. |
| 控制精度 | ±2 % | Precision of flow control for consistent cooling. |
| 响应时间 | ≤1 s | Fast response to changes in casting speed. |
| 电源 | 380–480 V AC | Three-phase, 50/60 Hz.IEC 60038 |
| 功率消耗 | 15–45 kW | Includes pumps and control system. |
| 防护等级 | IP54–IP65 | Protection against water and dust.IEC 60529 |
| 噪音水平 | ≤85 dB(A) | At 1 m distance.ISO 3744 |
| 重量 | 1500–3000 kg | Depends on configuration and materials. |
| 材料等级 | 304/316 | Stainless steel for corrosion resistance.ASTM A240 |
区间为行业参考值,供询价时圈定范围用,不构成供应商承诺。下单前请向法人制造商核实每一项数值与标准。
诱因 → 失效模式 → 工程缓解
| pressure: | 最高10 bar(系统工作压力) |
| flow rate: | 50-500 m³/h(冷却剂循环能力) |
| temperature: | 20-80°C(冷却剂温度范围) |
| slurry concentration: | 最高15%固体重量比(适用于浆料基系统) |
不是客户评论,也不是实时热度。以下维度用于前期 RFQ 准备和供应商评估。
这些分值是采购评估维度示例,不代表真实客户评分、具体国家买家反馈或实时询盘。
它在铸坯离开结晶器后控制冷却速率,确保适当凝固并防止缺陷。
水流量80–200 m³/h,压力0.4–0.8 MPa,喷嘴数量120–240个,区域长度3–6 m,坯料温度800–1100 °C。这些是参考范围,请确认您的型号。
不锈钢用于喷嘴和集管,碳钢用于管道和框架,铜合金用于喷嘴,聚合物/复合材料用于集管和密封件。
电源符合IEC 60038,防护等级符合IEC 60529,噪音符合ISO 3744,材料等级符合ASTM A240。请与制造商核实合规性。
CNFX 是开放目录,不是交易平台或采购代理。工厂资料和表单用于帮助你准备直接沟通。
CNFX 制造商资料、技术分类、公开产品信息和持续合理性检查。
说明目标数量、应用场景、交期和关键技术要求,用于准备 RFQ 或供应商评估。